2017 aluminium plate is rolled from a 2xxx series alloy in which copper is the principal alloying element, supported by additions of magnesium and manganese. It was one of the earliest high-strength aluminium alloys and remains a standard choice for machined components, rivets and general structural work where service temperature stays below about 150 °C.
Key Characteristics of Alloy 2017
Strength and heat resistance - the alloy performs well as a working material below 150 °C, and above roughly 125 °C it holds its strength better than higher-strength 7xxx grades.
Formability - good in the hot, annealed and freshly quenched conditions, so forming is carried out before natural ageing progresses and hardness rises.
Heat treatment response - strongly hardenable, but the cycle demands precise temperature and quench control to avoid distortion and scattered properties.
Corrosion resistance - limited in the bare condition; cladding with pure aluminium, anodising, chemical conversion coating or a paint system is used to protect exposed surfaces.
Welding - the high copper content makes fusion welding prone to cracking, so riveting and mechanical fastening are the usual joining methods.
Machinability and fatigue strength - clean chip formation and good fatigue behaviour suit machined parts that see repeated stress.
Chemical Composition of 2017 Aluminum
| Element | Composition range (wt.%) |
|---|---|
| Aluminium (Al) | Balance |
| Copper (Cu) | 3.5 – 4.5 |
| Magnesium (Mg) | 0.4 – 1.0 |
| Manganese (Mn) | 0.4 – 1.0 |
| Silicon (Si) | 0.2 – 0.8 |
| Iron (Fe) | 0.7 maximum |
| Zinc (Zn) | 0.25 maximum |
| Other elements, each | 0.05 maximum |
| Other elements, total | 0.15 maximum |
The trace-element rule is worth checking on every mill certificate: the limit is 0.05% maximum for each individual element and 0.15% maximum in total. Data sheets that reverse these two figures should be corrected before the alloy is approved for a project.
Mechanical and Physical Properties
| Property | Value |
|---|---|
| Density | 2.78 g/cm³ (0.100 lb/in³) |
| Melting range | 548 – 652 °C (1018 – 1206 °F) |
| Tensile strength | 275 – 435 MPa (40,000 – 63,000 psi) |
| Yield strength | 240 – 380 MPa (35,000 – 55,000 psi) |
| Elongation | 12 – 20% |
| Modulus of elasticity | 72 GPa (10.4 × 10⁶ psi) |
| Hardness | 55 – 120 HB; 95 – 150 HV |
| Electrical conductivity | 33 – 38% IACS |
| Thermal conductivity | 140 – 160 W/m·K |
The spread in strength reflects the temper supplied rather than scatter in the alloy itself, so the temper must always be stated with the order.
Temper Options: T4, T6, T451 and T651
| Temper | Treatment | Typical yield strength | Typical use |
|---|---|---|---|
| 2017 T4 | Solution heat treated and naturally aged to a stable condition | 35,000 – 40,000 psi (241 – 276 MPa) | Formed parts needing moderate strength with good machinability |
| 2017 T6 | Solution heat treated and artificially aged | 50,000 – 55,000 psi (345 – 379 MPa) | Structural components and high-stress parts |
| 2017 T451 | Solution heat treated, stress relieved by controlled stretching, naturally aged | 40,000 – 45,000 psi (276 – 310 MPa) | Aerospace and marine components needing stress-corrosion resistance |
| 2017 T651 | Solution heat treated, tensile stress relieved and artificially aged | 45,000 – 50,000 psi (310 – 345 MPa) | High-stress structural and precision-machined parts |
T4 delivers the best combination of formability and moderate strength; T6 raises strength and hardness at the cost of ductility; the stress-relieved T451 and T651 variants are chosen when machining stability and resistance to stress-corrosion cracking matter more than peak strength.
Available Sizes and Common Thicknesses
| Dimension | Range |
|---|---|
| Thickness | 3.175 mm (0.125 in) to 152.4 mm (6 in) and above |
| Width | 304.8 mm (12 in) to 1828.8 mm (72 in) and above |
| Length | 609.6 mm (24 in) to 3657.6 mm (144 in) or longer |
| Common plate thickness | Millimetre equivalent |
|---|---|
| 1/4 in | 6.35 mm |
| 3/8 in | 9.53 mm |
| 1/2 in | 12.7 mm |
| 3/4 in | 19.05 mm |
| 1 in | 25.4 mm |
Fabrication, Joining and Corrosion Protection
Riveting - the traditional joining method for 2017, with rivet temper and hole preparation matched to the plate thickness.
Welding - fusion welding tends to crack because of the copper-rich phases; where welding is unavoidable, filler selection and procedure qualification are essential.
Surface protection - cladding with pure aluminium, anodising, chemical conversion coating and paint systems all raise corrosion performance in aggressive environments.
Machining - the alloy machines freely and is widely used for screw-machine parts, fittings and brackets; sharp tooling and generous chip clearance keep surfaces clean.
Forming - hot forming, or forming in the annealed or freshly quenched state, avoids cracking in tight bends.
Typical Applications
Aerospace structural and machined parts where strength rather than corrosion resistance is the design driver.
Rivets and fasteners for airframe and general engineering assembly.
Automotive and transport components, including brackets, supports and turned parts.
Precision fittings, jigs and machine parts that operate at temperatures up to about 150 °C.
General engineering parts that will receive an anodised or painted finish before service.
Standards and Specification Notes
Sheet and plate are commonly ordered to ASTM B209, while JIS H4000 and GB/T 3190 together with GB/T 3880 cover chemical composition and dimensional requirements in other markets. For each order the certificate should record heat number, temper, chemistry, tensile results and dimensional inspection, so that plate can be traced from the ingot through to the finished machined part.
Frequently Asked Questions
Q: What is the difference between 2017 T4 and 2017 T6 aluminum plate?
T4 is solution heat treated and naturally aged at room temperature, which gives good formability with moderate strength. T6 is solution heat treated and then artificially aged in an oven, producing higher strength and hardness with lower ductility.
Q: Can 2017 aluminum plate be welded?
Fusion welding is not recommended because the copper content promotes hot cracking. Riveting, bolting and other mechanical fastening methods are the normal production routes; where welding cannot be avoided, a qualified procedure and suitable filler are required.
Q: How corrosion resistant is 2017 aluminum?
Bare 2017 has limited corrosion resistance compared with alloys such as 5052 or 6061. It performs acceptably in normal indoor atmospheres, but exposed or aggressive service demands cladding, anodising, chemical conversion coating or a paint system.
Q: Which temper should be selected if the part has to be formed first?
Form the plate in the annealed or freshly quenched condition and heat treat afterwards. Once natural ageing has progressed, ductility falls and tight forming operations risk cracking.
Q: Why is aluminium cladding used on 2017 sheet?
Rolling a thin layer of pure aluminium onto the surface creates a galvanic barrier that protects the copper-bearing core, which extends service life in outdoor and humid conditions without changing the underlying mechanical properties.
Q: What is the maximum service temperature for 2017 aluminum plate?
Roughly 150 °C for load-bearing working parts. Strength retention above 125 °C is better than that of 7075, which is why 2017 remains specified for moderately hot machinery components.
Q: How should 2017 plate be stored before machining?
Keep it flat, dry and clear of the floor, with spacing between plates to allow air movement. Protecting the surface from moisture and contact with dissimilar metals prevents staining and galvanic corrosion before the part is finished.