Position of 1xxx Coil in the Aluminium Family
Wrought aluminium is organised into eight alloy series. The 1xxx series is the commercially pure group: aluminium content is 99.0% or higher and the small quantities of iron and silicon present are controlled rather than deliberately added as hardening elements. Grades 1050, 1060 and 1100 are the three workhorses of that group, supplied as sheet, plate, strip and coil.
Their defining characteristics follow directly from the absence of alloying additions: high ductility, excellent electrical and thermal conductivity, outstanding corrosion resistance in most atmospheres, a bright reflective surface, and low mechanical strength that cannot be raised by heat treatment. They are work-hardened only.
Chemical Composition of 1050, 1060 and 1100
| Element | 1050 | 1060 | 1100 |
|---|---|---|---|
| Aluminium, min | 99.50% | 99.60% | 99.00% |
| Silicon | 0.25 max | 0.25 max | 0.95 max (Si + Fe) |
| Iron | 0.40 max | 0.35 max | 0.95 max (Si + Fe) |
| Copper | 0.05 max | 0.05 max | 0.05-0.20 |
| Manganese | 0.05 max | 0.03 max | 0.05 max |
| Magnesium | 0.05 max | 0.03 max | - |
| Zinc | 0.05 max | 0.05 max | 0.10 max |
| Titanium | 0.03 max | 0.03 max | - |
Limits follow GB/T 3190 and EN 573-3; ASTM B209 covers the same grades for sheet and plate. The only deliberate alloying addition in the group is the copper in 1100, and it is the reason 1100 is slightly stronger and slightly less conductive than 1050 or 1060.
Tempers and Available Dimensions
O: annealed, maximum ductility, used for deep drawing and spinning.
H12 / H14 / H16 / H18: quarter hard to full hard, produced by cold reduction, used for roofing, cladding, lithographic and general fabrication.
H22 / H24 / H26: the same strengths as the H1x series but stabilised and partially annealed, giving better formability at the same strength level.
Thickness: coils are commonly rolled from about 0.2 mm to 6 mm.
Width: typically 100 mm to 2650 mm depending on the mill; slitting to narrower widths is standard.
Coil form: inner diameter and coil weight are specified by the customer's decoiler, and when the customer will run a continuous line the coil must be ordered to the line's diameter.
Behaviour in Service and in the Workshop
Because the 1xxx grades cannot be strengthened by heat treatment, their strength comes only from cold work. That has practical consequences. A fully hard H18 coil is stiff and springy and needs more force to form, while an O temper coil forms easily but dents readily.
Electrical conductivity is high across the group, useful in busbars, cable sheathing and transformer parts.
Thermal conductivity supports use in heat exchangers, reflectors and cooking equipment.
Corrosion resistance is excellent in rural, urban and many chemical atmospheres, but the alloy is attacked by strong alkalis and by chlorides under wet contact conditions.
Weldability is good; gas tungsten arc and gas metal arc welding are used, and filler alloy 4043 or 1100 is typical for these grades.
Anodising produces a clear, bright oxide on 1050 and 1060; the copper in 1100 tends to give a greyer tone.
Where the Three Grades Are Used
| Grade | Typical applications |
|---|---|
| 1050 | Chemical equipment, lamp reflectors, food containers, cable sheathing, architectural flashings, sign blanks, deep drawn holloware |
| 1060 | Insulation jacketing, decorative trim, heat exchanger fins, transformer winding strip |
| 1100 | Chemical and food handling equipment, heat exchanger plates, spun holloware, storage tanks, decorative panels, general sheet metal work |
Storage, Handling and Quality Checks
Store coils horizontally on a dry mat or pallet, never directly on concrete, and keep them under cover.
Avoid condensation cycling; moisture trapped between laps causes white rust that cannot be removed by wiping.
Check the mill certificate for alloy, temper, dimensions and mechanical results, and verify composition limits against GB/T 3190 or EN 573-3.
Measure thickness across the width, not only at the centre; edge thinning is common on wide coils.
Test a sample for flatness, surface defects and, where the coil will be deep drawn, for earing and elongation.
Common Misconceptions
1xxx grades can be strengthened by heat treatment. They cannot; only cold work raises their strength.
The three grades are interchangeable. Purity differences change conductivity, anodised tone and strength, and 1100 contains copper.
A higher H number always means a better product. Harder temper means lower ductility, which may make the coil unusable for a forming operation.
Pure aluminium does not corrode. It resists most atmospheres well but is attacked by strong alkalis and by wet chlorides.
FAQ
Q: What is the difference between 1050 and 1060 aluminium coil?
Minimum aluminium content: 99.5% in 1050 and 99.6% in 1060. 1060 is marginally purer and softer, with a slightly lower permissible iron and manganese content.
Q: Is 1100 sheet stronger than 1050?
Slightly, because of the 0.05 to 0.20% copper addition, but the increase is modest and both remain low-strength, high-ductility materials.
Q: Which tempers are available in coils?
O, H12, H14, H16, H18, H22, H24 and H26 are standard, and other tempers can be produced to order.
Q: Can 1050 coil be welded?
Yes. Arc welding with a compatible filler gives sound joints, though the heat-affected zone loses the strength gained from cold work unless the design relies on the annealed properties.
Q: What is the maximum coil width?
It depends on the rolling mill; widths up to roughly 2650 mm are produced, with narrower widths supplied by slitting.
Q: How should aluminium coils be stored?
Horizontally, indoors, on a dry support, away from condensation and from contact with steel or copper, and rotated so that older stock is used first.