    5454 is an aluminum-magnesium alloy (5xxx series). Its European name is EN AW-5454 (AlMg3Mn).

     

    The H111 temper is an annealed condition with light strain hardening. The hardening is less than the H11 (1/8 hard) temper, so the material keeps good formability and machines easily, while its strength is a little above the fully annealed O temper. In short: H111 is a soft, formable temper, not a high-strength temper.

     

    GNEE is a China-based aluminum supplier. This page covers 5454-H111 aluminum plate and sheet - the sizes we supply, the mechanical properties, the common uses, and what to send us when you ask for a quote.

     

    Specification of 5454-H111 Aluminum Plate and Sheet

    Item

    Range

    Alloy

    5454

    Equivalent designation

    EN AW-5454 / AlMg3Mn, UNS A95454

    Temper

    H111 (also available: O, H22, H32, H34)

    Standard

    ASTM B209, EN 485, EN 14286

    Thickness

    0.3 – 200 mm

    Width

    100 – 2,500 mm

    Length

    500 – 12,000 mm (longer lengths available on request)

    Surface

    Mill finish, mirror finish

    5454-H111 Aluminum Plate5454-H111 Aluminum Plate for sale

     

    Size limits depend on thickness and the mill. If you need a specific size, send us the exact dimensions and quantity, and we will confirm what we can supply and at what tolerance.

    Contact Our Engineers Today

    Chemical Composition of 5454 Aluminum

    Per ASTM B209:

    Element

    Content (%)

    Magnesium (Mg)

    2.4 – 3.0

    Manganese (Mn)

    0.50 – 1.0

    Chromium (Cr)

    0.05 – 0.20

    Silicon (Si)

    0.40 max

    Iron (Fe)

    0.40 max

    Zinc (Zn)

    0.25 max

    Titanium (Ti)

    0.20 max

    Copper (Cu)

    0.10 max

    Others, each

    0.05 max

    Others, total

    0.15 max

    Aluminum (Al)

    Balance

     

    Mechanical Properties (typical minimums per ASTM B209)

    Temper

    Tensile strength (MPa)

    Yield strength (MPa)

    O

    215 – 285

    ≥ 85

    H111

    215 – 285

    ≥ 85

    H22

    250 – 305

    ≥ 180

    H32

    250 – 305

    ≥ 180

    H34

    270 – 325

    ≥ 200

    These are typical published values. Actual values depend on thickness. The Mill Test Certificate (MTC) for your order states the actual test results.

    Notes:

    H111 has about the same strength as the O temper. It is a forming temper, not a high-strength temper.

    H22 and H32 have similar strength. H32 is stabilized and more common in stock; H22 is available on request.

     

    Thickness Tolerances

    Thickness tolerances follow ASTM B209 and depend on the thickness and width combination. The table below shows typical symmetrical tolerances for common plate sizes.

    Thickness (mm)

    Width ≤ 1,250 mm

    Width 1,251 – 2,000 mm

    Width 2,001 – 2,500 mm

    0.50 – 3.00

    ±0.15 to ±0.20

    ±0.18 to ±0.25

    confirm

    3.01 – 6.00

    ±0.20 to ±0.30

    ±0.25 to ±0.35

    confirm

    6.01 – 12.00

    ±0.25 to ±0.40

    ±0.30 to ±0.45

    confirm

    12.01 – 25.00

    confirm

    confirm

    confirm

    These are typical ranges only. Send us your exact size and we will confirm the tolerance per ASTM B209 for your order.

     

    Main Properties of 5454-H111 Aluminum Plate

    Resistance to cracking during processing. 5454 has few brittle compounds, so it does not crack easily during cutting, forming, and machining. This matters for parts made to tight shapes.

    Good formability and stable welding. The soft H111 temper forms easily. Welding has a low tendency to crack, which gives cleaner weld joints.

    Good corrosion resistance. 5454 holds up well in humid and marine environments. This is the main reason it is used for tanks and structures that see moisture and chemicals.

     

    Common Uses Of 5454-H111 Aluminum Alloy Plate

    5454-H111 aluminum plate is used for parts that need to be formed, welded, and then exposed to moisture or chemicals:

    • Tanker truck tanks - body plates, baffles, and bulkheads
    • Tanks for transporting diesel, gasoline, and mild chemical liquids
    • Food industry tanks and equipment - cooking oil, juice, dairy
    • Boat and ship structures
    • General structural fabrication - frames, brackets, platforms

    For low-temperature (cryogenic) tanks, 5083 is the more common choice, because it keeps its toughness at very low temperatures. 5454 is a room-temperature and moderate-temperature material.

     

    Common Uses Of 5454-H111 Aluminum Alloy Plate

     

    Which Temper to Choose?

    5454 O - fully annealed, softest, best formability. For parts that need deep drawing or spinning.

    5454 H111 - light strain hardening, good formability, slightly stronger than O. A good default for parts that are formed before welding.

    5454 H22 - quarter hard, similar to H32 but not stabilized. Available on request.

    5454 H32 - quarter hard and stabilized, the common choice for tank bodies when you want more strength.

    5454 H34 - harder still, for parts that carry higher loads.

    The trade-off is simple: O and H111 form best; H22, H32, and H34 give more strength.

     

    Quality

    For every order we provide:

    Mill Test Certificate (MTC) with actual chemical composition and mechanical test results

    Dimensional and surface check before loading

    On request:

    Third-party inspection (SGS, BV, or other)

    Samples

    Certificate of origin

    GNEE ALUMINUM

    Dimensional and surface check before loading

     

    How to Get a Quote

    To get a price for 5454-H111 aluminum plate, send us:

    Alloy and standard (e.g., 5454, ASTM B209)

    Temper (H111, O, H22, H32, H34)

    Thickness, width, length

    Quantity (pieces or metric tons)

    Inspection and documentation needs (MTC, third-party inspection)

    Destination port

    GNEE handles material sourcing, production, inspection, documentation, and export packaging for 5454 aluminum plate orders. Send your specs and we will get back to you with price and lead time.

    packaging

     

    FAQ

    What is 5454 aluminum equivalent to?

    UNS A95454, EN AW-5454, and AlMg3Mn (ISO/EN designation) are the same alloy as 5454.

    Is 5454-H111 stronger than 5454-O?

    Marginally. H111 has light strain hardening, so it is a little stronger than O, but not much. For a real strength increase, choose H32 or H34.

    What is the difference between 5454 and 5052?

    5454 has more magnesium (2.4–3.0% vs 2.2–2.8%) and better resistance to stress corrosion cracking. For tanks and welded structures, 5454 is the stronger choice.

    What welding wire is used for 5454?

    Common filler wires are 5356 and 5183. Welding procedure tests on your actual batch are recommended before mass production.

    Can you supply small quantities or samples?

    Samples are usually available. For production orders, minimum order quantity depends on size and thickness - ask us and we will confirm.

    Get Project Quotation

    Hot Tags: 5454-h111 aluminum plate and sheet, China 5454-h111 aluminum plate and sheet manufacturers, suppliers, factory