5083 Tanker Aluminum Plate for Fuel, Oil & LNG Tanks
GNEE has supplied flat aluminum plate since 2008, with customers in more than 100 countries. As a 5083 tanker aluminum plate supplier and manufacturer, we operate rolling, leveling and cut-to-size lines focused on plate for transport equipment.
Fuel tanker aluminum plate, oil tank truck aluminum plate, LNG tanker aluminum plate and chemical tanker aluminum plate all start with the same alloy. With 4.0–4.9% magnesium and a density of 2.66 g/cm³ against 7.85 g/cm³ for steel, 5083 cuts shell weight sharply; H116 and H321 tempers are qualified for seawater service to ASTM B928 with ASTM G66 and G67 testing.
We supply O, H111, H112, H116, H321 and H32 tempers with cut-to-size lengths and mill-finish surfaces to ASTM B209, B928, EN 485-2 and GB/T 3880. Each batch carries an EN 10204 3.1 certificate.
Why 5083 Aluminum Plate Is Used for Tanker Bodies
A density of 2.66 g/cm³ against 7.85 g/cm³ for carbon steel is the first reason 5083 aluminum plate for tanker truck bodies is specified. A shell built to the same capacity carries roughly two thirds less structural mass, which raises usable payload over the working life of the vehicle.
Copper held to 0.10% maximum limits the potential difference between the aluminum matrix and cathodic particles. That control slows galvanic attack where the tank body bolts to steel brackets or meets road salt, which extends inspection intervals in service.
Welded joints retain usable strength in the as-welded condition, with weld-metal tensile values near 275 MPa and joint efficiencies of 0.7–0.85. Fabricators size seams against a defined design strength and place large shells into service without a post-weld heat-treatment step.
The highest strengths in the 5xxx plate family come from solid-solution strengthening by 4.0–4.9% magnesium combined with work hardening. As a non-heat-treatable alloy, 5083 reaches 305 MPa minimum tensile strength in H116 and H321 while staying formable into shell sections.
Elongation of at least 16% in O temper lets fabricators roll cylindrical shells and press dished heads in a single forming sequence. Baffles, manways and end caps draw from the same plate stock, which simplifies material planning for a complete tank build.


Chemical Composition of 5083 Aluminum Plate
Actual heat chemistry per Mill Test Certificate, sourced to ASTM B209 / EN 573-3 / GB/T 3190.
| Element | Limit, wt% (ASTM B209 / EN 573-3 / GB/T 3190) |
|---|---|
| Si | ≤0.40 |
| Cu | ≤0.10 |
| Mg | 4.0–4.9 |
| Zn | ≤0.25 |
| Mn | 0.40–1.00 |
| Ti | ≤0.15 |
| Cr | 0.05–0.25 |
| Fe | ≤0.40 |
| Others, each | ≤0.05 |
| Others, total | ≤0.15 |
| Al | Remainder |
Mechanical Properties of 5083 Aluminum Plate
| Temper | Standard, thickness | Rm, MPa | Rp0.2, MPa | A |
|---|---|---|---|---|
| O / H111 | ASTM B209M, 1.2–40 mm | 275–350 (min 275) | 125–200 (min 125) | ≥16% |
| O / H111 | EN 485-2, 3–12.5 mm | 270–350 (min 270) | ≥115–125 | ≥15–16% |
| H112 | ASTM B209M, 6.3–40 mm | ≥275 | ≥125 | ≥12% |
| H116 | ASTM B928, 3–40 mm | ≥305 | ≥215 | ≥10% |
| H321 | ASTM B928, 3–40 mm | 305–385 (min 305) | ≥215 | ≥10–12% |
| H32 | ASTM B209M, 4.8–38 mm | 305–385 (min 305) | ≥215 | ≥12% |
Physical and Thermal Properties of 5083 Aluminum Plate
| Property | Typical value |
|---|---|
| Density | 2.66 g/cm³ |
| Elastic modulus | ~70–71 GPa |
| Melting range | 570–640°C |
| Thermal conductivity | ~110–140 W/(m·K) |
| Coefficient of thermal expansion | 23–25×10⁻⁶/K |
| Electrical conductivity | ~29–30% IACS |
| Specific heat | ~900 J/(kg·K) |
| Poisson's ratio | ~0.33 |
These reference values support tank weight estimates, expansion allowances at shell-to-head joints and heat-transfer calculations for heated or cryogenic cargoes.
5083 Aluminum Plate and Sheet Specifications
| Category | Description |
| Alloy / Temper | 5083 Aluminum, 5083 H111, 5083 H116, 5083 H321, 5083 H32, 5083 H34, 5083 H22, 5083 O, AA5083, EN AW 5083, AL 5083 H112, AL 5083 O |
| Product Type | 5083 Aluminum Plate, 5083 Aluminum Sheet, 5083 Tooling Plate, 5083 Cast Aluminum Plate, 5083 Aluminum Armor Plate |
| Applications | Welding components, Marine and Shipbuilding, Armor Plate, Tooling and Molds, Structural Components |
| Standards / Certification | ASTM 5083, ASTM B928, EN 5083, EN AW 5083, QQ-A250/6 |
| Thickness (inches) | 0.01", 0.118", 0.236", 0.250", 0.5", 1" (customizable 1 mm – 200 mm) |
| Width (inches) | 36", 48", 60", 72" |
| Length (inches) | 48", 96", 118", 120", 144" |
| Finish | Mill Finish, Anodized, Color Coated, PVDF Coated, Mirror, Brushed, Embossed, Checkered, Stucco Embossed |
A 6mm 5083 aluminum plate for tanker shells is a common balance of weight and stiffness, with 4–6 mm frequent in production. Wider plate panels let a fabricator reduce longitudinal welded seams, and cut-to-size blanks arrive matched to the drawing.
Deviation from nominal dimensions follows ANSI H35.2(M)-2000. When an order names ASTM B209, EN 485-3 or EN 485-4, the corresponding tables govern, and the agreed deviation is written into the contract for the specific gauge and panel size.
International Grade Equivalents for 5083 Aluminum Plate
| Designation | System |
|---|---|
| AA 5083 | Aluminum Association |
| UNS A95083 | Unified Numbering System |
| EN AW-5083 | European designation |
| AlMg4.5Mn0.7 | EN chemical designation |
| WNr 3.3547 | Werkstoff number |
| JIS A5083 | Japanese Industrial Standard |
| GB/T 5083 (formerly LF4) | Chinese designation |
| AMS-QQ-A-250/6 | Plate material specification |
These grades are compositionally similar; cross-grade substitution requires MTC and design approval. One governing standard and temper should be named on the purchase order.
Aluminum Plate Tempers for Tankers: H111 vs H116 vs H321
H116 and H321 share the 5083 composition and the same minimum tensile strength of 305 MPa with 215 MPa yield. H116 is produced in the stabilized as-rolled condition on the rolling line; H321 receives a low-temperature stabilization step after rolling.
Elongation separates the two in practice: H321 holds ≥12% within the ASTM B928 band while H116 is specified at ≥10%. A 5083 H321 aluminum plate is chosen where the shell sees sustained heat, since the stabilization step improves resistance to sensitization in long service.
A 5083 H111 aluminum plate for tanker shells offers ≥16% elongation and easier forming of dished heads and complex baffles. H111 suits ambient-temperature fuel and chemical cargoes where the plate is formed after delivery.
Plate held above 65°C in service, or mounted close to exhaust and heating equipment, moves to H321 or to alloy 5454. 5083 H116 and H321 retain toughness at cryogenic temperatures down to −162°C and below, which supports LNG tank service subject to design approval.
| Tank area | Temper | Typical gauge | Selection basis |
|---|---|---|---|
| Fuel tank shell | H111 / H116 | 4–8 mm | Formability with corrosion resistance |
| LNG cryogenic tank | H116 / H321 | 4–10 mm | Low-temperature stability |
| Chemical tank shell | H116 / H321 | 4–10 mm | Cargo compatibility and corrosion allowance |
| Dished end caps | O | equal to or thicker than shell | Deep drawing with added head thickness |
| Baffles and swash plates | O / H111 | 3–6 mm | baffle gauge follows the tank design |
| Zones above 65°C or near heat sources | 5454 or H321 | 4–8 mm | Sensitization resistance under sustained heat |
Heads are equal to or thicker than the shell, with one gauge step commonly added for forming. Baffle gauge follows the tank design and typically sits about 1 mm below the shell gauge. Final values come from the fabrication drawing.

Service Temperature and Sensitization of 5083 Aluminum Plate
Sustained exposure above approximately 65°C drives beta phase Al₃Mg₂ to precipitate along grain boundaries in 5xxx aluminum plate. That precipitation path creates susceptibility to intergranular attack, exfoliation and stress-corrosion cracking on a heated tank shell.
ASTM G66 (ASSET) and ASTM G67 (NAMLT) are the acceptance tests used to qualify H116 and H321 product under ASTM B928 / B928M. Both tests run on the delivered temper, so the temper is fixed at the time of the material order.
Where a cargo or cleaning cycle keeps the shell above 65°C, alloy 5454 or an internal liner is specified. Ambient and cryogenic services stay with 5083 H111, H116 or H321.
| Service condition | Material route | Basis |
|---|---|---|
| Ambient fuel and chemical cargoes | 5083 H111 / H116 | Corrosion and forming performance |
| Cryogenic LNG service | 5083 H116 / H321 | Low-temperature stability |
| Intermittent heat near 65°C | 5083 H321 | Stabilized temper |
| Sustained service above 65°C | 5454 or lined 5083 | Sensitization resistance |
Welding and Fabrication of 5083 Aluminum Plate
ER5183 and ER5356 are the standard filler wires for 5083 aluminum plate; ER5556 is available where higher weld-metal strength is required. MIG and TIG both suit shell seams, and 5183 filler gives a close strength and color match to the parent plate.
As-welded tensile strength lands near 275 MPa with joint efficiencies of 0.7–0.85. Welded tanks enter service in the as-welded condition, with local heat-affected-zone softening included in the welded-joint design check.
Heat input and interpass temperature are controlled to limit sensitization in multi-pass seams. Groove faces are cleaned to remove oxide before welding, using dedicated stainless brushes and solvents on the joint preparation.
Plate is sheared, plasma-cut, rolled and leveled with standard aluminum workshop equipment. Cut edges on tank panels are deburred before fitting.
5083 vs 5454 Aluminum Plate for Tanker Bodies
For buyers comparing 5083 vs 5454 aluminum plate for tanker bodies, the decision rests on magnesium level, service temperature and shell strength.
| Alloy | Mg, % | Density, g/cm³ | Typical temper | Rm, MPa | Rp0.2, MPa | High-temperature retention | Tank role |
|---|---|---|---|---|---|---|---|
| 5052 | 2.2–2.8 | 2.68 | H32 | ~230 | ~180 | Moderate | Liners and small fittings |
| 5754 | 3.0–3.6 | 2.66 | H111 | ~260 | ~170 | Moderate | Baffles and lighter tanks |
| 5454 | 2.4–3.0 | 2.66 | H111 / H32 | ~275 | ~200 | Strong above 65°C | Heated asphalt and bitumen tanks |
| 5086 | 3.5–4.5 | 2.66 | H116 / H321 | ~300 | ~215 | Good | Marine-service candidate in H116/H321, subject to ASTM B928 / B928M and G66 / G67 review |
| 5083 | 4.0–4.9 | 2.66 | H111 / H116 / H321 | ≥305 | ≥215 | Good to about 65°C | Primary tank shell and heads |
5083 is the main shell alloy where strength and corrosion allowance govern. H116 and H321 are the seawater-service tempers qualified under ASTM B928 / B928M with ASTM G66 and G67 testing. 5454 is selected for sustained service above 65°C, 5052 and 5754 serve non-load-bearing parts, and 5086 requires design review.
Standards and Classification for 5083 Aluminum Plate
Standards are applied in the order set by the purchase order and the tank design code:
| Standard | Scope for tank plate |
|---|---|
| ASTM B928 / B928M | H116 and H321 plate with exfoliation and intergranular corrosion requirements |
| ASTM B209 / B209M | General plate in O, H111, H112 and H32 |
| EN 485-2 / EN 485-3 | Mechanical properties and dimensional tolerances |
| EN 573-3 | Chemical composition limits |
| GB/T 3880 / GB/T 3190 | Plate product and composition designation |
| ASME SB-209 | Plate for ASME-coded pressure equipment projects |
| AMS-QQ-A-250/6 | Plate material designation for cross-reference |
| EN 13094 / ADR | Dangerous-goods transport tank compliance framework |
EN 485-1 and EN 485-4 supply general and dimensional conditions, and EN 515 defines temper designation. EN 14286:2008 covers weldable rolled aluminum products of 3–12 mm for transportable pressure equipment and dangerous-goods tanks, matching common tank shell gauges.
EN 13094 and ADR set the compliance framework for dangerous-goods transport tanks; material and inspection records are assembled to the project design code.
Classification society certificates from CCS, DNV, ABS, LR, BV, NK and KR are available on request per project.
Each batch is released with EN 10204 3.1 MTC.
3.2 certification and third-party inspection are arranged when the order specifies them.
Quality Inspection of 5083 Aluminum Plate
Spectroscopic chemical analysis against the ordered standard, recorded on the MTC.
Tensile and yield testing at the delivered temper and gauge.
Thickness, width, length and flatness checks on produced plate.
Surface inspection for rolling marks, scratches and edge condition.
Ultrasonic testing carried out when the purchase order calls for it.
Heat-to-plate batch traceability from cast heat to finished plate.
Third-party inspection arranged for 3.2 certificates or buyer witness points.




Packaging of 5083 Aluminum Plate
Each plate is wrapped in waterproof paper and plastic film, placed on a wooden pallet and secured with steel strip. Desiccant is added for sea freight, and the stack is secured inside the container or break-bulk hold. Final packing is confirmed against the discharge port and container type on the order.

Processing Services for 5083 Aluminum Plate

Cut-to-size shearing and plate sawing for shell and head blanks.

Slitting and edge trimming, including mill edge and rolled edge.

Leveling and flattening of rolled plate before forming.

Gauge and panel grouping by tank zone so one order covers shell, heads and baffles.
About GNEE
Established in 2008 as a flat-rolled aluminum plate supplier, with shipments to more than 100 countries.
Rolling, leveling and cut-to-size equipment assigned to plate production.
Tank-grade product released with EN 10204 3.1 MTC and traceable heat numbers.
Export packing planned against discharge port, container type and cargo routing.
Engineering support for temper selection, gauge grouping and drawing-based panel cutting.
Request a Quote for 5083 Tanker Aluminum Plate
Request a quote for 5083 tanker aluminum plate. Send the temper, thickness, width, length, quantity, destination port and any named standard or classification requirement.
Commercial terms: MOQ is flexible, with small trial orders and full containers both accepted. Lead time runs 15–30 days, an EN 10204 3.1 MTC ships with the goods, and pricing is benchmarked to SMM.
Our team returns a quotation within 24 hours.
FAQ
Q: Which EN, GB and JIS designations match 5083 plate on a tank order?
A: The usual equivalents are EN AW-5083 (AlMg4.5Mn0.7, WNr 3.3547), UNS A95083, JIS A5083 and GB/T 5083, formerly LF4. These grades are compositionally similar; cross-grade substitution requires MTC review and design approval. State one governing standard on the purchase order and match each delivery to it.
Q: Which temper should I specify for tank shells, end caps and baffles?
A: Fuel tank shells are commonly ordered in H111 or H116 at 4–8 mm, with 4–6 mm frequent in production. Dished end caps take O temper and are equal to or thicker than the shell, while baffle gauge follows the tank design at O or H111. Where the shell sees sustained heat near 65°C, specify H321 or alloy 5454.
Q: Does 5454 replace 5083 for a fuel tanker running above 65°C?
A: 5083 carries more magnesium and reaches higher strength, while sensitization limits long-term service near 65°C. 5454 holds its mechanical properties better under sustained heat and is the usual choice for heated asphalt or bitumen tanks. Apply the temperature threshold to the actual shell condition, including cleaning cycles.
Q: What thickness tolerance and cut-to-size options are available?
A: Plate is supplied from 0.3–200 mm thick, 100–2500 mm wide and up to 6000 mm long, with cut-to-size blanks produced to your drawing. Dimensional deviations follow ANSI H35.2(M)-2000, and ASTM B209 or EN 485-3/-4 tables apply when the order names those standards. Final tolerances are recorded in the contract.
Q: Which filler alloy and joint efficiency apply to 5083 tank welds?
A: ER5183 and ER5356 are the common fillers for MIG and TIG welding of 5083 plate, with ER5556 available for higher weld strength. As-welded tensile strength is around 275 MPa and joint efficiency falls in the 0.7–0.85 band. Welded tanks enter service without post-weld heat treatment.
Q: What documents and classification certificates ship with each batch?
A: Every batch ships with an EN 10204 3.1 Mill Test Certificate listing heat chemistry and mechanical results. Corrosion-test data and batch traceability are added when the order calls for them. Classification society certificates from CCS, DNV, ABS, LR, BV, NK and KR are arranged on request per project.
Q: What minimum order quantity and lead time should I plan for?
A: MOQ is flexible: small trial orders and full containers are both accepted, so a tank prototype and a production run follow the same inquiry route. Standard lead time is 15–30 days from order confirmation, with the schedule fixed against gauge, temper and any cut-to-size work.
Q: Will H116 and H321 plate meet ASTM B928 corrosion requirements?
A: ASTM B928 defines the exfoliation and intergranular corrosion requirements for 5083 H116 and H321 plate. Qualification is verified by ASTM G66 ASSET and ASTM G67 NAMLT testing on the delivered temper, and results are reported with the batch documents when the purchase order specifies them.
Q: How does cut-to-size plate reduce the number of tanker weld seams?
A: Plate supplied at the rolled panel length lets a fabricator form a longer shell section, which removes intermediate circumferential joints and shortens the longitudinal seam. Wider plate covers more of the shell circumference, so fewer panels are joined and less welding time is spent per tank.
Hot Tags: 5083 aluminum plate for tanker truck, China 5083 aluminum plate for tanker truck manufacturers, suppliers, factory