HENAN GNEE NEW MATERIAL CO., LTD
86-372-5055135

Why 7075 Aluminum Is Called Steel-Like

Dec 26, 2025

Export Control Notice - These Grades Cannot Be Exported

7075 aluminum - including forged 7075-T6 - falls within these categories and is not available for export.

High-strength aluminum alloys of this class are listed under the export control regulations of the People's Republic of China for dual-use items and technologies. Shipping them out of China requires an export licence issued by the competent Chinese authorities. In practice a licence is not obtained for ordinary commercial orders in these categories, so GNEE does not export them.

GNEE does not export to any party or destination prohibited under applicable export control and international sanctions laws.

Control status technically turns on six variables: alloy grade, temper, product form, dimensions, quantity and intended end-use. Whatever the combination, none of the grades in the table below are available for export from GNEE.

Aluminum grades affected by these controls

Alloy grade Common temper(s) Tensile strength (MPa) - reference
7075 T6 / T651 540 – 570
7075 T73 / T7351 485 – 500
7075 T76 / T7651 500 – 515
7050 T7451 / T6 475 – 620
2024 T351 / T4 425 – 470
7A04 T6 ≥ 530
2014 T6 approx. 460 – 500
2017 T4 approx. 390 – 480 (some specifications may reach higher)
2195 - approx. 572
7068 - approx. 623
7055 - approx. 654
7150 - approx. 643

Strength values in this table are indicative reference ranges used for control classification. They are not specification minimums. The governing limits for any enquiry come from the applicable standard or your drawing.

What we can quote instead

We cannot accept export enquiries for the grades listed above. If strength is the reason you are looking at them, send us the load case, the service environment and the fabrication method, and we will quote a non-controlled substitute - usually from the 5xxx or 6xxx series - with properties that fit the job and no export restriction attached.

 

What Makes 7075 Steel-Like

Within the wrought aluminum alloy system, 7075 represents the practical upper limit of strength achievable with conventional aluminum alloys. While maintaining a relatively low density of about 2.81 g/cm3, its mechanical performance rivals many low-carbon steels, which is why engineers describe 7075-T6 as steel-like aluminum. Compared with common alloys such as 6061, 7075 shows dramatically higher yield and tensile strength, making it indispensable in aerospace, defense and high-performance engineering where weight reduction is critical and components face extreme stress concentrations.

Alloy System and Strength Mechanism

7075 belongs to the 7xxx series, an Al-Zn-Mg-Cu system developed specifically to maximize strength. Zinc, typically 5.1-6.1% by weight, is the dominant alloying element; combined with magnesium and copper it enables the formation of MgZn2 precipitates during heat treatment. These precipitates create a dense internal barrier that resists dislocation movement, producing strength levels far beyond those of Mg2Si-based alloys such as 6061. In short, 7075 is not an upgraded 6061 but a fundamentally different alloy optimized for strength at the expense of manufacturability.

How the T6 Temper Creates Peak Strength

Maximum strength is achieved through precipitation hardening in three stages: solution heat treatment dissolves the alloying elements, rapid quenching traps them in a supersaturated state, and artificial aging allows controlled precipitation of the strengthening phases. This microstructure maximizes strength but significantly reduces ductility. The T6 temper delivers peak strength, while the T73 over-aging temper sacrifices roughly 10-15% of strength to dramatically improve resistance to stress corrosion cracking in corrosive environments.

Mechanical and Physical Properties

7075-T6 provides yield strength up to about 465 MPa and tensile strength up to about 540 MPa in typical tempers, with an elastic modulus of about 71.7 GPa and thermal conductivity around 130 W/mK. A key design note is that 7075 is much stronger than 6061 but not significantly stiffer: strength prevents permanent deformation, while stiffness controls elastic deflection. The alloy's high strength comes with higher machining forces and increased material cost.

Stress Corrosion and Temper Selection

The T6 temper increases susceptibility to stress corrosion cracking in corrosive environments. Aerospace engineers often specify 7075-T73 where long-term corrosion resistance matters, and T651 is strongly recommended for machined parts because the controlled stretching step relieves internal residual stress and prevents distortion during CNC machining. For any corrosive or long-term stressed service, surface protection such as anodizing or conversion coating should be planned.

Typical Applications

7075 is used in aircraft wing spars, fuselage frames and landing gear components, defense housings, racing suspension arms and chassis plates, climbing hardware, high-end bicycle components, and short-run injection molds from T651 plate. It is not a general-purpose alloy; it is selected only when its strength advantage clearly outweighs its limitations in corrosion resistance, weldability and machining cost.

FAQ

Q: Why is 7075 called steel-like aluminum?

A: Because its strength approaches many low-carbon steels while weighing about one-third as much, thanks to its Al-Zn-Mg-Cu system and precipitate strengthening.

Q: How strong is 7075-T6?

A: Typical values reach yield strength up to about 465 MPa and tensile strength up to about 540 MPa, among the highest of conventional aluminum alloys.

Q: Is 7075 stronger than 6061?

A: Yes, by a large margin, but 6061 offers better weldability, corrosion resistance, machinability and lower cost.

Q: Which temper should I use for machined parts?

A: T651 is recommended for CNC machining because the controlled stretch relieves residual stress and prevents distortion.

Q: Does 7075 resist corrosion well?

A: General corrosion resistance is lower than many alloys, and T6 is more prone to stress corrosion cracking; use T73 or protective coatings for corrosive service.