HENAN GNEE NEW MATERIAL CO., LTD
86-372-5055135

Core Properties of 3003-H14 Aluminium: Composition, Strength and Fabrication

Dec 15, 2025

Alloy and Temper Definition

3003 is an aluminium-manganese alloy in which manganese is the principal addition, at 1.0 to 1.5%, with copper held between 0.05 and 0.20%. Because the strengthening comes from solid solution and strain hardening rather than from a precipitate, 3003 is non-heat-treatable: it cannot be hardened by quenching and ageing, and its properties after welding remain close to those of the annealed condition in the weld zone.

The H14 temper is the half-hard condition in the standard work-hardening sequence, which runs H12 for quarter hard, H14 for half hard, H16 for three-quarter hard and H18 for full hard. H14 is therefore a deliberately intermediate choice, offering roughly double the strength of the annealed temper while retaining enough ductility for bending, roll forming and moderate drawing.

Composition and Property Data

Composition is normally specified to ASTM B209 or to the EN 573-3 composition standard, with corresponding mechanical requirements in ASTM B209 or EN 485-2. The table below summarises the data a buyer can work from.

Parameter Value Basis
Manganese 1.0 to 1.5% Standard composition limits
Copper 0.05 to 0.20% Standard composition limits
Tensile strength, H14 145 to 195 MPa EN 485-2 for this temper
0.2% proof strength, H14 125 MPa minimum EN 485-2 for this temper
Elongation, H14 Low single figures to about 10%, depending on gauge Typical for a half-hard temper
Density 2.73 g/cm3 Typical physical data
Melting range About 643 to 654 degrees Celsius Typical physical data
Thermal conductivity Approximately 190 W/mK Typical physical data

The high thermal conductivity relative to steel is one of the reasons 3003 is used in heat exchanger and cooking applications: heat spreads quickly and hot spots do not develop locally. Density is marginally higher than for a pure aluminium grade because of the manganese addition.

Corrosion Behaviour

3003 has good resistance to atmospheric corrosion and offers useful resistance to many neutral and mildly acidic foodstuffs, which is why it dominates cookware, food containers and catering foil. Unlike the higher-magnesium 5xxx grades it is less resistant to salt water, so it is not the preferred choice for marine hardware. The alloy is not normally specified for strongly alkaline or strongly acidic chemical service, where a protective coating or a different alloy family is required.

In food-contact applications the material is supplied against the applicable national standard for metal food-contact materials, and a lacquer or a compatible coating is applied where the food is acidic or salty.

Forming, Welding and Finishing

In the H14 temper 3003 bends readily, and a minimum inside bend radius of roughly one times the sheet thickness is a reasonable design starting point for a 90 degree bend across the rolling direction; tighter radii should be validated on production tooling, and the risk of cracking increases when the bend line runs parallel to the rolling direction. Deep drawing is usually carried out from the O or H12 temper and the part hardens as it is formed.

3003 is readily welded by gas tungsten arc and gas metal arc processes using a 4043 filler, and it can also be joined by resistance welding. The heat of welding anneals the material locally, reducing strength in the affected zone, so a welded joint should not be designed to develop the full H14 strength of the parent sheet. Brazing and soldering are straightforward with appropriate flux, and the alloy responds well to anodising, which produces a clear film with good hardness.

Typical Applications and Selection Notes

Application Why 3003-H14 fits
Food containers and trays Formability, food-contact suitability, thermal conductivity
Heat exchanger fins and tubes Conductivity, corrosion resistance, ease of joining
Roofing and cladding sheet Atmospheric corrosion resistance, moderate strength
Signage and nameplates Flat, uniform surface, good anodising response
Chemical equipment and ductwork Corrosion resistance and ease of fabrication

Where higher strength is required without a heat treatment, 5052 is the usual upgrade; where higher strength is required in a heat-treatable alloy, 6061 replaces 3003 at the cost of weld strength retention and forming flexibility.

Frequently Asked Questions

Q: Is 3003 a heat-treatable alloy?
A: No. Its strength comes from manganese in solid solution and from strain hardening, so it cannot be strengthened by solution treatment and ageing.

Q: What does the H14 temper mean?
A: It is the half-hard condition in the standard work-hardening sequence, between H12 quarter hard and H16 three-quarter hard, giving roughly double the strength of the annealed temper.

Q: How much manganese does 3003 contain?
A: Between 1.0 and 1.5%, with copper held between 0.05 and 0.20% under the standard composition limits.

Q: Can 3003-H14 be welded?
A: Yes, with a 4043 filler using standard arc processes, but welding locally anneals the material, so the joint should not be designed to develop full parent metal strength.

Q: Why is 3003 used for cookware and food containers?
A: It combines good formability, useful resistance to neutral and mildly acidic foodstuffs and high thermal conductivity, which spreads heat evenly and avoids hot spots.

Q: What is the usual upgrade when more strength is needed?
A: 5052 for a non-heat-treatable, weldable upgrade, or 6061 where a heat-treatable alloy is acceptable despite reduced weld zone strength.