HENAN GNEE NEW MATERIAL CO., LTD
86-372-5055135

Common Types of 1060 Aluminum Plate Processing and How to Choose Them

Jul 31, 2025

1060 aluminum plate is a commercially pure wrought grade that is cut, bent, drawn, welded and finished into busbars, reflectors, heat sink plates and enclosures. Its behaviour during each of those operations follows directly from its purity and temper.

What Makes 1060 Aluminum Plate Easy to Process

1060 contains a minimum of 99.6% aluminum, which places it among the purest grades in common mill supply. Because there are almost no alloying elements to restrict the movement of dislocations, the plate is soft, extremely ductile and highly conductive. Density is about 2.705 g/cm3, thermal conductivity is roughly 234 W/(m·K) at 20 °C and electrical conductivity is around 61% IACS. The nominal melting range is 646 to 657 °C, which gives a comfortable window for welding and brazing. The designation 1060 is used in the American and Chinese systems, while the nearest European designation is EN AW-1050A with a 99.5% minimum aluminum content; the two are similar in behaviour but should not be treated as interchangeable on a certificate of analysis.

Property Typical value Effect on processing
Aluminum content 99.6% minimum Keeps ductility and conductivity high, limits strength
Density About 2.705 g/cm3 Light parts, but lower stiffness than steel
Thermal conductivity About 234 W/(m·K) at 20 °C Suits heat sinks and cold plates
Electrical conductivity About 61% IACS Suits busbars and transformer windings
Melting range 646 to 657 °C Defines the welding and brazing window
Tempers supplied O, H12, H14, H18, H24 Strength is set by cold work, not by heat treatment

Cutting and Blanking Routes

Because 1060 is supplied both as thin sheet and as heavy plate, the first processing decision is normally the cutting method. Guillotine shearing is the most economical route for straight edges on sheet up to about 6 mm, but soft material tends to smear, so correct blade clearance and sharp tooling matter more here than on a hard alloy. Laser cutting produces accurate profiles and tight nesting for thicknesses up to roughly 8 mm; the high reflectivity of pure aluminum means the machine must be run with adequate power and correct focus to avoid dross on the underside. Abrasive waterjet cutting leaves no heat-affected zone and is therefore preferred for thick plate or for parts that will be anodized afterwards, since there is no recast layer along the cut edge. For high volumes, blanking dies and rotary slitting replace single-part cutting, and burrs are removed with a deburring roller or a linishing pass. Whichever route is used, edges should be free of embedded abrasive and loose oxide before welding, because trapped contamination is a frequent cause of porosity.

Bending, Roll Forming and Deep Drawing

The outstanding ductility of 1060 is the reason it appears in lighting reflectors, kitchenware and curved decorative panels. On a press brake the minimum inside bend radius for the softer tempers approaches the sheet thickness, and bends are easier to control when they run across the rolling direction rather than parallel to it. Roll forming produces long, uniform sections such as reflector housings and trim profiles, and because springback is small in the annealed condition the tooling can be set once and run consistently. Deep drawing and spinning convert flat blanks into lamp housings, cookware and enclosures. When a part needs more than one draw, an intermediate anneal restores ductility between passes, and a light lubricant film prevents the sheet from galling the die. Since cold working strengthens 1060 quickly, the incoming temper and the number of forming steps are planned together rather than decided separately.

Annealing and Temper Control

Cold working raises the strength of 1060 and reduces its elongation, and annealing reverses that effect. A full anneal to the O temper is carried out at roughly 340 to 350 °C with sufficient soak time for complete recrystallization, while a partial or process anneal at a lower temperature relieves internal stress and still leaves some stiffness behind. Because the alloy cannot be strengthened by solution treatment, the H tempers such as H12, H14, H18 and H24 are produced by controlled cold reduction from the annealed condition. H18 is fully hard rolled sheet with the highest strength and the least elongation, whereas H24 is strain hardened and partially annealed, which gives a practical balance for parts that still have to be formed after delivery. Annealing records should capture temperature, soak time and cooling method, because uneven cooling leaves residual stress that appears later as distortion during machining or as poor flatness after anodizing.

Welding and Surface Finishing

1060 welds readily by TIG or MIG with 1100 or 4043 filler wire, and gas welding is also used for thin sheet. Because the base metal is soft and conducts heat away quickly, heat input has to be controlled to prevent burn-through, and fixtures hold long seams flat while they cool. Riveting, clinching and adhesive bonding are common alternatives where welding heat would spoil a finished face. For appearance work, the plate is brushed, polished or bright dipped and then anodized. High-purity grades form a clear, transparent anodic film, so the final appearance depends almost entirely on how well the surface beneath it was prepared; polishing marks and scratches remain visible through the coating. Powder coating and chemical conversion coatings are used where colour or extra corrosion protection is required. Parts for outdoor or humid service should be finished on cut edges as well as on the flat faces, because exposed edges corrode first.

Matching the Processing Route to the Application

Application Usual temper Main processing steps Reason
Lighting reflector O or H24 Blanking, spinning or drawing, polishing, anodizing Soft temper takes curvature; clear anodic film
Busbar and transformer winding O or H12 Slitting, shearing, bending, edge deburring Conductivity around 61% IACS with easy bending
Heat sink and cold plate H14 or H24 Cutting, CNC machining, brazing High conductivity with usable stiffness
Signage and advertising board H14 or H24 Cutting, bending, brushing, coating Flatness and uniform surface appearance
Kitchenware O Deep drawing, spinning, intermediate anneal, polishing High elongation for deep draws
Architectural cladding panel H14 to H24 Roll forming, bending, anodizing Formability with consistent finish
Nameplate and dial plate H18 Blanking, printing Fully hard sheet holds flatness

Frequently Asked Questions

Q: What is 1060 aluminum plate normally used for?
It is used for busbars, transformer windings, heat sink plates, lighting reflectors, signage, kitchenware and decorative panels, wherever high conductivity and easy forming matter more than strength.

Q: Can 1060 aluminum plate be strengthened by heat treatment?
No. The grade responds only to cold work, so it is supplied in the O condition or in H tempers such as H12, H14, H18 and H24 rather than in T tempers.

Q: Is 1060 the same as 1050A?
They are close but not identical. 1060 guarantees 99.6% minimum aluminum, while EN AW-1050A guarantees 99.5%, so the difference matters when a specification calls for a certified purity level.

Q: Which temper should be specified for bending?
O and H12 bend most easily, H14 and H24 are used where some stiffness is needed, and bends should run across the rolling direction with an inside radius close to the sheet thickness.

Q: How does 1060 aluminum plate behave during anodizing?
It forms a clear anodic film, which means the result mirrors the preparation of the base surface; thorough polishing and a clean rinse sequence are essential before the anodizing tank.

Q: Does 1060 aluminum plate weld easily?
Yes, TIG and MIG welding with 1100 or 4043 filler work well, provided heat input is limited on thin sheet and the welded assembly is restrained to control distortion.