HENAN GNEE NEW MATERIAL CO., LTD
86-372-5055135

6061 Aluminum Plate and Sheet: Properties, Temper and Uses

Oct 20, 2025

What Is 6061 Aluminum Plate and Sheet

6061 is a heat-treatable 6000-series (Al-Mg-Si) alloy supplied as rolled sheet and plate, and also as strip, rod, bar, tube, wire, forgings and extruded structural shapes. In the T6 and T651 tempers it combines moderate-to-high strength with excellent corrosion resistance, good weldability and easy machining, which is why it is one of the most widely specified general-purpose aluminum products in industrial fabrication.

T651 is the same composition and temper as T6, with one extra operation: after quenching, the plate is stretched by a controlled amount to relieve internal stress. That step improves dimensional stability, so T651 plate machines flatter and distorts far less than standard T6 plate when large amounts of metal are removed. Sheet and plate in this alloy are commonly used for aircraft fixtures, electrical fixtures, communications equipment, automated mechanical parts, precision machining, mold manufacturing, electronics and precision instruments, SMT stencils and PC board solder carriers, as well as structural framing, base plates, gussets, marine hardware and automotive components.

Chemical Composition and Metallurgical Structure

The principal alloying elements are magnesium and silicon, which combine to form magnesium silicide (Mg2Si). Because Mg2Si is soluble in the aluminum matrix, the alloy responds strongly to artificial age hardening, and this is the basis of the T6 temper. Typical composition ranges are given below.

Element Content (wt.%) Function
Si 0.40-0.80 Forms Mg2Si with magnesium
Mg 0.80-1.20 Principal strengthening element
Cu 0.15-0.40 Raises strength without seriously reducing corrosion resistance
Cr 0.04-0.35 Offsets the harmful effect of iron
Mn ≤0.15 Controls grain structure and iron-bearing phases
Fe ≤0.70 Impurity; kept low for ductility and finish
Zn ≤0.25 Impurity; small additions increase strength
Ti ≤0.15 Grain refinement
Others Each ≤0.05, total ≤0.15 Residual limits
Al Balance Matrix

Chromium and manganese counteract the negative effect of iron on toughness and finish. Small amounts of copper or zinc increase strength without a large penalty in corrosion resistance. Titanium or zirconium is used to refine grains and control recrystallization, and lead and bismuth are added in free-machining variants to improve chip breaking. The result is a dense, defect-free material that polishes well and takes a uniform anodic oxide film with good coloring response.

Mechanical Properties and Available Tempers

6061 cannot match the strength of the 2XXX or 7XXX families, but its balance of properties is unusually broad: good formability in the annealed condition, reliable strength after aging, and stable behaviour under welding and machining. The table below lists representative room-temperature values for the tempers most often ordered.

Temper Tensile strength Yield strength (0.2%) Elongation Hardness
6061-O (annealed) approx. 115 MPa (17 ksi) approx. 48 MPa (7 ksi) approx. 25% approx. 30 HB
6061-T4 approx. 241 MPa (35 ksi) approx. 145 MPa (21 ksi) approx. 22% approx. 65 HB
6061-T6 approx. 310 MPa (45 ksi) approx. 275 MPa (40 ksi) approx. 12% approx. 95 HB
6061-T651 approx. 310 MPa (45 ksi) approx. 275 MPa (40 ksi) approx. 12% approx. 95 HB

Other physical values useful for design work: density 2.70 g/cm3, modulus of elasticity 68.9 GPa (10,000 ksi), fatigue strength around 96 MPa (14 ksi) at 5 x 10^8 cycles, and thermal conductivity of about 167 W/m.K at 25 °C. All of these figures refer to plate and sheet in the T6 or T651 temper unless stated otherwise, and they are typical rather than guaranteed minimum values.

Standard Sizes, Tolerances and Surface Options

Temper: T1, T2, T3, T4, T6, T651 and others on request

Thickness: 0.2-350 mm

Width: 30-2600 mm

Length: 200-11000 mm

Mother coil: continuous cast (CC) or direct chill (DC) cast feedstock

Surface: clean and smooth, free of bright speck, corrosion, oil staining and slitting marks

Protection: paper interlayer, white film, blue film, black-white film or micro-bound film

Delivery: about 30 days after receipt of deposit, depending on temper and size

Sheet and plate are produced and inspected against international specifications including GB/T 3880, EN 485, EN 573, ASTM B209 and JIS H 4000. Buyers should always state the governing standard, temper and tolerance class on the purchase order, because thickness tolerance, flatness and edge condition differ between these standards.

Heat Treatment, Applications and Alloy Selection

Aging practice depends on the product form. Sheet, plate, rolled or cold-rolled wire, rod, bar and drawn tubing are aged at a metal temperature of 160 °C (320 °F) for 18 hours. Extruded rod, bar, profiles and tube, die forgings, hand forgings and rolled rings are aged at 175 °C (345 °F) for 8 hours. Holding to these cycles, rather than shortcutting them, is what produces the published T6 properties.

Because 6061 extrudes easily and rolls cleanly, it is available as sheet, strip, plate, rod, forging stock, tube, pipe, wire, extruded profiles and structural shapes. The same alloy therefore turns up in machinery frames, hydraulic manifolds, truck bodies, tower structures, ship and tram fittings, railway car components, mold plates, jigs and fixtures, and precision instrument housings.

When choosing between common alternatives: 6063 extrudes to a brighter, smoother finish and is preferred for architectural trim, windows and doors, while 6061 provides higher strength for structural work. 5052 contains magnesium as its main addition, welds exceptionally well and resists marine atmospheres, but it is not heat treatable, so its strength comes only from cold work. 2024 is stronger and fatigue resistant because of its copper content, yet it machines less easily, welds poorly and needs protection in corrosive service. For an all-round alloy that is predictable, weldable, readily available and reasonably priced, 6061 remains the default choice.

Frequently Asked Questions

Q: What is the difference between 6061-T6 and 6061-T651 plate?
Both have the same chemical composition and the same T6 temper. T651 plate is additionally stretched after quenching to relieve internal stress, which gives better dimensional stability when the part is heavily machined.

Q: Is 6061 aluminum heat treatable?
Yes. It is an age-hardenable Al-Mg-Si alloy. Solution heat treatment followed by artificial aging at 160 °C for 18 hours develops the T6 temper and the published strength level.

Q: Can 6061 aluminum be welded?
Yes, it has very good weldability and is suitable for structures that require frequent welding. Filler alloys of the 4043 or 5356 type are normally used, and strength in the heat-affected zone is reduced by welding unless the assembly is re-aged.

Q: What thickness can be supplied?
Thickness runs from 0.2 mm up to 350 mm, with widths of 30-2600 mm and lengths of 200-11000 mm in either CC or DC mother coil. Non-standard sizes can be cut to order.

Q: How does 6061 compare with 5052?
6061-T6 is roughly twice as strong and can be heat treated, while 5052 is more formable, superior for welding and slightly better in marine corrosion resistance. Choose 5052 for formed, welded panels and 6061 where strength and machinability matter.

Q: Does 6061 corrode in outdoor service?
It has excellent resistance to atmospheric corrosion and forms a natural protective oxide. Anodizing or painting further improves appearance and durability in aggressive or marine environments.