1060 Aluminum Plate vs 3003 Aluminum Plate

Oct 23, 2025

Key Differences

Properties:

1060 Aluminum Plate: Known for its high purity (99.6% aluminum), excellent electrical conductivity, and corrosion resistance.

3003 Aluminum Plate: An aluminum-manganese alloy, providing moderate strength and superior corrosion resistance, especially in moist environments.

Property 1060 Aluminum Plate 3003 Aluminum Plate
Alloy Composition 99.6% Al Al + Mn
Strength Low Moderate
Corrosion Resistance Good Good, enhanced with Mn
Formability Excellent Good
Weldability Good Good
Machinability Excellent Slightly lower
Surface Finish Smooth Smooth
Cost Lower Slightly higher
Applications Signage, appliances, reflectors, cooking utensils, chemical equipment Automotive parts, cookware, storage tanks, sheet metal work
Tensile Strength 60-95 MPa 110-205 MPa
Yield Strength Below 70 MPa 40-150 MPa
Density ~2.7 g/cm³ ~2.73 g/cm³
Work Hardening Low Higher
Heat Treatment Non-heat-treatable Non-heat-treatable
Availability Readily available Readily available
Anodizing Ability Poor Better
Electrical Conductivity Excellent Slightly lower

6063-aluminum-sheet

Alloy Composition:

1060 Aluminum Plate: Contains 99.6% pure aluminum, with minimal traces of silicon and other elements.

3003 Aluminum Plate: Contains aluminum and manganese, offering improved strength and corrosion resistance compared to 1060.

Characteristics:

1060: Excellent electrical and thermal conductivity, high corrosion resistance, especially in environments without significant chemical exposure.

3003: Moderate strength, excellent formability, and outstanding corrosion resistance, especially in humid environments, and is also weldable.

Strength:

1060: Lower strength, making it suitable for applications where strength is less critical.

3003: Offers better strength due to alloying elements, making it more appropriate for applications needing moderate strength.

Corrosion Resistance:

Both alloys are resistant to corrosion, but 3003 is slightly superior due to the addition of manganese.

Formability:

1060: Known for its excellent formability, ideal for creating complex shapes or for deep drawing processes.

3003: Offers good formability but slightly lower than 1060, still suitable for various forming processes.

Weldability:

Both alloys can be easily welded with conventional methods like TIG, MIG, and resistance welding.

Machinability:

1060: Easier to machine due to its lower strength, allowing for easier cutting, drilling, and milling.

3003: Slightly more challenging to machine due to the alloying elements but still relatively easy to process.

Surface Finish:

Both alloys achieve a smooth surface, though 1060 may have a slight edge due to its higher purity. Both can be rolled, polished, or anodized to enhance both aesthetics and protection.

Cost:

1060: Generally more affordable than 3003 because of its simpler composition and the greater availability of raw materials.

3003: Slightly more expensive due to the addition of manganese, which increases production costs.

Applications:

1060: Common in signage, appliances, reflectors, cookware, and chemical equipment, particularly where lightweight and corrosion resistance are required.

3003: Frequently used in automotive parts, cookware, storage tanks, and general sheet metal work where moderate strength and corrosion resistance are needed.

Tensile Strength:

1060: Ranges from 60 to 95 MPa, depending on processing and tempering.

3003: Offers higher tensile strength, ranging from 110 to 205 MPa due to the alloying elements.

Yield Strength:

1060: Yield strength is generally below 70 MPa, indicating its lower strength.

3003: Ranges from 40 to 150 MPa, suitable for structural applications requiring medium strength.

Density:

1060: Has a density of approximately 2.7 g/cm³.

3003: Slightly denser at around 2.73 g/cm³.

Work Hardening:

1060: Low work hardening rate, meaning its strength doesn't increase much with cold working processes like rolling or bending.

3003: Higher work hardening rate, enabling increased strength through cold working operations.

Heat Treatment:

Both alloys are non-heat-treatable, meaning their mechanical properties cannot be improved by heat treatment methods such as annealing.

Anodizing Ability:

3003: More suitable for anodizing compared to 1060, resulting in better surface finish and corrosion resistance after anodization.

Electrical Conductivity:

1060: Known for its excellent electrical conductivity, making it suitable for electrical applications like conductors and busbars.

3003: Has slightly lower electrical conductivity than 1060, but still sufficient for many electrical applications.